| Inconel Alloy | US $10/Pound |
Useful Topics
Inconel ASTM Standard & Specification
Products Available Shapes |
International Standard |
|---|---|
Bar |
ASTM B 446/ASME SB 446, ISO 9723, VdTÜV 499, BS 3076NA21, EN 10095, DIN 17752 , ASME Code Case 1935, SAE/AMS 5666, |
Wire |
DIN 17753, SAE/AMS 5837, ISO 9724 |
Sheet / Plate |
ASTM B 443/ASTM SB 443,ISO 6208, VdTÜV 499, BS 3072NA21 (Sheet, Plates), EN 10095, DIN 17750, ASME Code Case 1935, SAE/AMS 5599 & 5869 & MAM 5599, |
| Pipe / Tube | ASTM B444/ B829, ASME SB 444/ SB 829 (Seamless), ASME SB 704/SB 751 and ASTM B704/B 751 (Welded), ASME SB 705/ SB 775 and ASTM B705/B 775 (Welded), VdTÜV 499, BS 3074NA21 (Seamless), ISO 6207, SAE/AMS 5581 (Seamless & Welded), DIN 17751, ASME Code Case 1935. |
Pipe Fittings (Buttweld) |
ASTM B 366/ ASME SB 366 |
Forging/ Forged Items |
ASTM B 564/ ASME SB 564, DIN 17754, ISO 9725 |
Welding Wire |
A5.14 ERNiFeCr-2 |
| Heat Resisting Steels & Alloys | DIN 17744, ISO 4955A |
Inconel Alloy Temperature Range
| Inconel 600 Heat Capacity units | Metric: 0.444 J/g-°C |
| Inconel 625 Heat Capacity units | Metric: 0.41 J/g-°C English: 0.098 BTU/lb-°F |
| Inconel | Element, proportion by mass (%) | ||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Ni | Cr | Fe | Mo | Nb & Ta | C | Co | Cu | Mn | Al | Ti | Si | S | P | B | |
| 600 | ≥72.0 | 14.0–17.0 | 6.0–10.0 | ≤0.15 | N/A | ≤0.5 | ≤1.0 | ≤0.5 | ≤0.015 | ||||||
| 617 | 44.2–61.0 | 20.0–24.0 | ≤3.0 | 8.0–10.0 | 0.05–0.15 | 10.0–15.0 | ≤0.5 | ≤0.5 | 0.8–1.5 | ≤0.6 | ≤0.5 | ≤0.015 | ≤0.015 | ≤0.006 | |
| 625 | ≥58.0 | 20.0–23.0 | ≤5.0 | 8.0–10.0 | 3.15–4.15 | ≤0.1 | ≤1.0 | ≤0.5 | ≤0.4 | ≤0.4 | ≤0.5 | ≤0.015 | ≤0.015 | ||
| 690 | ≥58 | 27–31 | 7–11 | ≤0.05 | ≤0.50 | ≤0.50 | ≤0.50 | ≤0.015 | |||||||
| Nuclear grade 690 | ≥58 | 28–31 | 7–11 | ≤0.04 | ≤0.10 | ≤0.50 | ≤0.50 | ≤0.50 | ≤0.015 | ||||||
| 718 | 50.0–55.0 | 17.0–21.0 | Remainder | 2.8–3.3 | 4.75–5.5 | ≤0.08 | ≤1.0 | ≤0.3 | ≤0.35 | 0.2–0.8 | 0.65–1.15 | ≤0.35 | ≤0.015 | ≤0.015 | ≤0.006 |
| X-750 | ≥70.0 | 14.0–17.0 | 5.0–9.0 | 0.7–1.2 | ≤0.08 | ≤1.0 | ≤0.5 | ≤1.0 | 0.4–1.0 | 2.25–2.75 | ≤0.5 | ≤0.01 | |||
| Products | Hardness, Rockwell | Form and Condition | Yield Strength | Tensile Strength | Elongation % | ||
|---|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | ||||
| Bars | 65-85B | Cold drawn Annealed | 25-50 | 170-345 | 80-100 | 550-690 | 55-35 |
| Plates | 65-85B | Hot rolled Annealed | 30-50 | 205-345 | 80-100 | 550-725 | 55-35 |
| Sheets | 88B max | Cold Rolled (CR) Annealed | 30-45 | 205-310 | 80-100 | 550-690 | 55-35 |
| Pipe/ Tubes | 88B max | Cold Drawn Annealed | 25-50 | 170-345 | 80-100 | 550-690 | 55-35 |
| Wires | - | Cold Drawn Annealed | 35-75 | 240-520 | 80-120 | 550-830 | 45-20 |
| Wires | - | Cold Drawn No 1 Temper | 70-105 | 480-725 | 105-135 | 725-930 | 35-15 |
| Wires | - | Spring Temper | 150-210 | 1035-1450 | 170-220 | 1170-1520 | 5-2 |
| Bars/ Rods | ≤ 287 HB | Annealed | 60 | 414 | 120 | 827 | 30 |
| Sheet | 145-240 | Annealed | 60 | 414 | 120 | 827 | 30 |
| Tube | - | Annealed | 60 | 414 | 120 | 827 | 35 |
Inconel has a higher melting point of 2,540°F-2,600°F (1,390°C-1,425°C), check below the grade wise melting range.
| Inconel 718 Melting Point Range | Solution Treated: 2500-2600 Deg F Solution Treated and Aged: 1370-1430 Deg C |
| Inconel 601 Melting Point Range | 1411 Deg C (2571 Deg F) |
| Inconel 600 Melting Point Range | Metric: 1354 - 1413 Deg C English: 2470 - 2580 Deg F |
| Inconel 625 Melting Point Range | 2350 - 2460 Deg F (1280 - 1350 Deg C) |
Corrosion Resistant + High Temp Strength alloys