Hastelloy C276

Hastelloy Alloy C276

Hastelloy C276 composition, Alloy C276 price per kg

Check Hastelloy C276 ASTM Standard, Alloy C276 properties, EFAB approved Hastelloy C276 material manufacturers

Hastelloy C276 Products

Hastelloy Alloy C276 price per kg

Alloy C276 Price US $40/Kg

Hastelloy Alloy C276 ASTM Standard

ASTM B564, B574, B575, B619, B622, B626, B366, B462, B775

Specification of Hastelloy C276

UNS Designation Number: N10276

W.Nr. Number (DIN): 2.4819

HASTELLOY® C-276 alloy
(N10276, W10276)
Sheet, Plates & Strips B 575 / SB 575
P= 43
Billet, Rods & Bars B 574 / SB 574
P= 43
Coated Electrode SFA 5.11/ A 5.11 (ENiCrMo-4)
DIN 2.4887
(EL-NiMo15Cr15W)
F= 43
Bare Welding Rod and Wires SFA 5.14/ A 5.14 (ERNiCrMo-4)
DIN 2.4886
(SG-NiMo16Cr16W)
F= 43
Pipes & Tubes - Seamless B 622 / SB 622
P= 43
Pipes & Tubes -Welded B 619 /SB 619
P= 43
Pipe Fittings B 366 / SB 366
P= 43
Forging Products B 564 / SB 564
P= 43
DIN 17744 No. 2.4819 NiMo16Cr15W
TÜV Werkstoffblatt 400
Kennblatt 320
Kennblatt 319
Other Stanard NACE MR0175
ISO 15156

Hastelloy C276 equivalent material

UNS EN WERKSTOFF NR. (WNR) AFNOR JIS BS GOST
N10276 NiMo16Cr15W 2.4819 – NW 0276 – ХН65МВУ

Hastelloy C276 Temperature Range

HASTELLOY® C-276 alloy
( W10276 / N10276)
ASME Section l 1000°F (538°C)1
Section lll Class 1 -
Class 2 800°F (427°C)2
Class 3 800°F (427°C)2
Section Vlll Div. 1 1250°F (677°C)3
Div. 2 1250°F (677°C)3
Section Xll 650°F (343°C)3
B16.5 1250°F (677°C)4
B16.34 1250°F (677°C)5
B31.1 1000°F (538°C)6
B31.3 1250°F (677°C)7
VdTÜV (doc #) 844°F (450°C)8,
#400

Hastelloy Alloy C276 Applications & Uses

  • Chemical processing plats
  • Expansion bellows
  • Nuclear fuel plants
  • Electric power industry
  • Nuclear reactors
  • Industrial equipment manufacturers

Hastelloy C276 Composition

Grade % Ni W Cr Fe Co C Mo Mn S Si V P
C

Min.

balance 3 14.5 4     15          
Max. 4.5 16.5 7 2.5 0.08 17 1 0.03 1 0.35 0.04
C276 Min. balance 3 14.5 4     15          
Max. 4.5 16.5 7 2.5 0.01 17 1 0.03 0.08 0.35 0.04

Properties of Hastelloy Alloy C276

Physical properties

Density 8.9 g/cm³
Melting point 1325-1370 ℃

Minimum mechanical properties in the room temperature

Alloy state Yield strength R P0. 2N/mm² Tensile strength
Rm N/mm²
Elongation
A 5 %
C /C276 283 690 40

Other Relevant Grades

HASTELLOY C276 UNS N10276 | W.NR. 2.4819

Excellent corrosion resistance material

whatsapp chat